Nā Pōmaikaʻi o ka Uea Molybdenum i Hoʻohui ʻia me Lanthanum

ʻOi aku ke kiʻekiʻe o ka mahana recrystallization o ka uea molybdenum lanthanum-doped ma mua o ka uea molybdenum maʻemaʻe, a no ka mea hiki i ka liʻiliʻi o La2O3 ke hoʻomaikaʻi i nā waiwai a me ke ʻano o ka uea molybdenum. Eia kekahi, hiki i ka hopena lua o La2O3 ke hoʻonui i ka ikaika o ka uea molybdenum i ka mahana o ka lumi a hoʻomaikaʻi i ka brittleness o ka mahana o ka lumi ma hope o ka recrystallization.

Hoʻohālikelike Mahana Hoʻohou Hou: Ua hoʻonui maopopo ʻia ka microstructure o ke kaula molybdenum maʻemaʻe ma 900 ℃ a hoʻohou hou ʻia ma 1000 ℃. Me ka piʻi ʻana o ka mahana annealing, hoʻonui pū ʻia nā hua recrystallization, a emi nui nā ʻiʻo fibrous. Ke hiki ka mahana annealing i 1200 ℃, ua hoʻohou hou ʻia ke kaula molybdenum, a hōʻike kāna microstructure i kahi mau hua recrystallized like. Ke piʻi ka mahana, ulu like ʻole ka hua a ʻike ʻia he mau hua coarse. Ke hoʻohou hou ʻia ma 1500 ℃, maʻalahi ka haki ʻana o ke kaula molybdenum, a hōʻike kona ʻano i ka hua coarse equiaxed. Ua hoʻonui ʻia ke ʻano fiber o ke kaula molybdenum i hoʻopili ʻia me ka lanthanum ma hope o ka hoʻohou hou ʻia ma 1300 ℃, a ua ʻike ʻia ke ʻano niho ma ka palena o ke kaula. Ma 1400 ℃, ua ʻike ʻia nā hua recrystallized. Ma 1500 ℃, ua emi nui ke ʻano o ka fiber, a ua ʻike maopopo ʻia ke ʻano o ka recrystallized, a ua ulu like ʻole nā ​​​​hua. ʻOi aku ke kiʻekiʻe o ka mahana recrystallization o ka uea molybdenum lanthanum-doped ma mua o ka uea molybdenum maʻemaʻe, ʻo ia hoʻi ma muli o ka hopena o nā ʻāpana lua o ka La2O3. Hoʻopilikia ka lua o ka La2O3 i ka neʻe ʻana o ka palena o ka palaoa a me ka ulu ʻana o ka palaoa, a laila e hoʻonui ai i ka mahana recrystallization.

Hoʻohālikelike ʻana i nā ʻano mīkini o ka mahana o ka lumi: Hoʻonui ʻia ka elongation o ke kaula molybdenum maʻemaʻe me ka piʻi ʻana o ka mahana annealing. Ke piʻi ka mahana anneal ma 1200 ℃, hiki ka elongation i ka waiwai kiʻekiʻe loa. Hoʻemi ʻia ka elongation me ka piʻi ʻana o ka mahana anneal. Hoʻoheheʻe ʻia ma 1500 ℃, a ua aneane like kona elongation me ka ʻole. Ua like ka elongation o ke kaula molybdenum La-doped me ke kaula molybdenum maʻemaʻe, a hiki ka nui o ka elongation i ka nui loa ke hoʻoheheʻe ʻia ma 1200 ℃. A laila emi ka elongation me ka piʻi ʻana o ka mahana. ʻO ka ʻokoʻa wale nō ka lohi o ka wikiwiki hōʻemi. ʻOiai ua lohi ka elongation o ke kaula molybdenum lanthanum-doped ma hope o ka annealing ma 1200 ℃, ʻoi aku ka kiʻekiʻe o ka elongation ma mua o ke kaula molybdenum maʻemaʻe.


Ka manawa hoʻouna: Dec-19-2021